J. Ocean Eng. Technol. 1995;9(1):92-100.    

A Study on Fatigue Crack Propagation Behavior with Pure-Ti Plate
순수 티타늄 판재의 피로균열 전파거동에 관한 연구
오세욱,김태형,김득진,임만배
동아대학교 기계공학과,동아대학교 생산기술연구소,동아대학교 대학원,동아대학교 대학원
© 1995 The Korean Society of Ocean Engineers     Open access / Under a Creative Commons License
Keywords: Anisotropy, Fatigue crack propagation behavior, Fatigue crack opening-closing behavior, Effective stress intensity factor range, Fracture ductility, Forward plastic zone, Reversed plastic zone
핵심용어: 이방성, 피로균열진전거동, 피로균열 개,폐구 거동, 유효응력확대계수폭, 파단연성, 전방 소성역, 역 소성역
Abstract
The effect of different anisotropy and stress ratio on fatigue crack propagation behavior was investigated under various stress ratio(R=-0.4, -0.2, 0.2, 0.2, 0.4) using pure titanium sheet used in aerospace, chemical and food industry. The rack closure behavior under constant load amplitude fatigue crack propagation test was examined. Fatigue crack propagation rate da/dN was estimated in terms of effective stress intensity factor range, $Delta$K$_{eff}$, regardless of various stress ratio but was influenced by anisotropy. Also, it was found that the effect of anisotropy was considerably decreased but still not negligible when he da/dN was evaluated by a conventional parameter, $Delta$$K_{eff}$/E and when the modified da/dN.$sqrt{varepsilon}_f$ was evaluated by $Delta$$K_{eff}$/E. On the other hand, da/dN could be evaluated uniquely by effective new parameter, $Delta$K$_{eff}$/$sigma_{ys}$, regardless of anisotropy, as int he following equation da/dN= C"[$frac{DeltaK_{eff}}{sigma_{ys}}$] n". And effective stress intensity factor range ratio, U was estimated by the following equation with respect to the ratio of reversed plastic zone size, $Delta r_{p}$ to monotonic plastic zone size, $r_p$ regardless of stress ratio and anisotropy. U=-4.45$(Delta r_{p}/r_{p})^{2}$+4.1$(Delta r_{p}/r_{p})$+0.245_{p})$+0.245


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY

Browse all articles >

PUBLICATION ETHICS
FOR CONTRIBUTORS
Editorial Office
President Office BD Rm. 1302, 13 Jungang-daero 180beon-gil, Dong-gu, Busan 48821, Republic of Korea
Tel: +82-51-759-0656    Fax: +82-51-759-0656    E-mail: ksoehj@ksoe.or.kr                

Copyright © 2024 by The Korean Society of Ocean Engineers.

Developed in M2PI

Close layer
prev next